Skip to main content

KOVAR parts cold working manufacturing process

KOVAR parts are precision processed by CNC numerical control machine tools and used for electronic industry equipment; precision parts processing, swiss machining, CNC precision parts processing.



(1) Eliminate machining stress.

When Kovar undergoes plastic deformation during cold working, about 10% to 15% of the applied energy is converted into internal energy, which is commonly referred to as internal stress, so that the Kovar machining material structure is in an unstable state. Under this condition, it can be maintained for a long time without significant changes.

Once it is heated, a series of changes in structure and properties will occur, and the material structure tends to a stable state. This change in structure and properties, especially changes in the structure of the structure, is reflected on the sealing surface.

The tensile stress on the molybdenum group glass during high temperature sealing may cause the glass to produce small cracks and leak air.

(2) Eliminate work hardening.

In the process of cold working, cnc manufacturing and forming of Kovar parts, due to defects such as grain elongation and grain breakage in the internal material structure, crystal defects and dislocation density increase greatly. The smaller the distance between the dislocation and the dislocation, the greater the interference between each other, and the greater the distortion of the surrounding lattice.

Each dislocation line has a stress field, and the dislocation and dislocation pass through each The interaction of the stress field causes the hardness and elasticity of Kovar to increase, while the plasticity decreases, which is work hardening.

If the work hardening is not eliminated, the stress field of the interaction between dislocations and dislocations will be broken due to crystal recovery or recrystallization during high-temperature sealing, and the balance will be lost. This also affects the sealing of alloy machining and glass. Certain stress effects.

Comments

Popular posts from this blog

What are the characteristics of the CNC turning process?

What are the characteristics of the CNC turning process? Turning is a method of cutting the workpiece on the lathe by rotating the workpiece relative to the tool. Turning is the most basic and common cutting processing method. Most workpieces with revolving surfaces can be processed by turning methods, such as inner and outer cylindrical surfaces, inner and outer conical surfaces, end surfaces, grooves, threads, and rotary forming surfaces. Common lathes can be divided into horizontal lathes, floor lathes, vertical lathes, turret lathes and profiling lathes, and most of them are horizontal lathes.

The Influence of CNC Turning and Milling Machining on Turning Efficiency

The cutting efficiency of CNC lathes will be affected by human factors, environmental factors and the machine tool itself. Let's talk about the influence of cutting amount and cutting tools on CNC lathe processing among many factors.   Reasonable cutting amount can improve the efficiency of CNC lathe. When the   laser  cutting  speed is increased by 10 times and the feed rate is increased by 20 times, far beyond the traditional cutting forbidden zone, the cutting mechanism has undergone a fundamental change.   The result of CNC turning  and milling combined processing is: the metal removal rate per unit power is increased by 30% to 40%, the cutting force is reduced by 30%, the cutting life of the tool is increased by 70%, and the cutting left on the workpiece is greatly reduced. Heat, cutting vibration almost disappeared; cutting processing has taken an essential leap. According to the current situation of CNC lathes, increase the feed per tooth, improve pr...

Machining and welding process notes for TC4 titanium alloy parts

Common welding methods for titanium and titanium alloys are as follows: Argon arc welding, submerged arc welding, vacuum electron beam welding, etc. Tungsten argon arc welding is used for thicknesses of 3 mm or less, and argon arc welding is done for 3 mm or more. The purity of argon is over 99.99%, and the content of air and water vapor in argon is strictly controlled. Currently, for TC4 titanium alloys, argon arc welding, plasma arc welding are often used for welding, but both methods need to be filled with welding material. Limitations on shield gas, purity and effectiveness increase the oxygen content of the joint, reduce its strength and increase its post-weld deformation. Electron beam welding and laser beam welding are used. The following is a description of precision welding and precautions for TC4 titanium alloy. 1. Weld hole problem Table of Contents 1. Weld hole problem 2, internal quality of welded part 3. Weld depth and its variation 4, j...